Research Article
Galvanic Corrosion and Fatigue Behavior of a SM480C Welded Joint Steel in a Sea-Crossing Suspension Bridge
Table 3
Fatigue test results of bridge deck specimens.
| Average thickness (mm) | Load amplitude (kN) | Actual stress amplitude (MPa) | Nominal stress amplitude (MPa) | Number of cycles () |
| ≈6.0 | 20.7 | 230 | 115 | | ≈8.0 | 20.7 | 172 | 115 | | ≈9.0 | 15.5 | 115 | 86.1 | | ≈9.0 | 20.7 | 153 | 115 | | ≈10.0 | 20.7 | 138 | 115 | | ≈10.5 | 27.1 | 172 | 150 | |
|
|