Research Article

In Situ Monitoring of Corrosion under Insulation Using Electrochemical and Mass Loss Measurements

Figure 8

SEM images of corroded SS after 7 days’ CUI tests with 3.5 wt% NaCl solutions. (a) IW at 93°C, (b) CW at 93-50°C.
(a)
(b)