Study on Impact Mechanical Properties of Reentrant Bionic Automotive Energy Absorbing Box
| Parameters | Volume forming rate (L/hr) | Scanning speed (m/s) | Build cavity temperature (°F) | Laser power (W) | Powder layer thickness (mm) |
| Tensile sample | 76 | 7.8 | 6,400 | 31 | 0.1 |
|
|