Research Article
Mechanical Parameters and Post-Cracking Behaviour of HPFRC according to Three-Point and Four-Point Bending Test
Table 7
Four-point bending tests: tensile strength parameters.
| | | | | | | | | kN | MPa | MPa | MPa | — | — |
| DS1%_1 | 26.3 | 7.2 | 10.5 | 12.0 | 1.5 | 1.1 | DS1%_2 | 24.6 | 6.7 | 11.6 | 13.2 | 1.7 | 1.1 | DS1%_3 | 24.7 | 6.7 | 11.1 | 12.3 | 1.7 | 1.1 | Mean value | 25.2 | 6.9 | 11.1 | 12.5 | 1.6 | 1.1 | DS2%_1 | 25.6 | 7.0 | 17.4 | 22.3 | 2.5 | 1.3 | DS2%_2 | 26.3 | 7.2 | 16.0 | 21.2 | 2.2 | 1.3 | DS2%_3 | 25.6 | 7.0 | 15.3 | 17.4 | 2.2 | 1.1 | Mean value | 25.8 | 7.1 | 16.2 | 20.3 | 2.3 | 1.2 |
|
|