Research Article
Assessing Mechanical Properties of Hot Mix Asphalt with Wire Wool Fibers
Table 5
Effect of adding wire wool on the creep properties of the mix.
| Property | Wire wool percentage | 0.0% | 0.25% | 0.50% |
| Core temperature (°C) | 23.38 | 23.68 | 24.05 | Contact stress (KPa) | 9 | 9 | 9 | Deviator stress (KPa) | 207 | 207 | 207 | Dynamic load (KN) | 1.641 | 1.506 | 1.594 | Permanent deformation (mm) | 0.445 | 0.844 | 0.151 | Resilience deformation (mm) | 0.031 | 0.0354 | 0.044 | Accumulated strain (%) | 0.445 | 0.844 | 0.151 | Resilient strain (%) | 0.031 | 0.036 | 0.044 | Resilient modulus (MPa) | 1051.99 | 559.183 | 465.708 | Creep modulus (MPa) | 41.68 | 23.665 | 135.411 |
|
|