Research Article
Study on Material Properties of Magnesium Oxide Carbonized Prestressed Pipe Piles
Table 4
Mass loss rate of active magnesium oxide carbonized block after freeze-thaw.
| | Numbering | Quality before freezing and thawing (g) | Quality after freezing and thawing (g) | Loss rate (%) |
| | D1 | 362.1 | 357.3 | 1.33 | | D2 | 358.9 | 356.7 | 0.61 | | D3 | 375.2 | 371.4 | 1.01 | | D4 | 365.4 | 362.3 | 0.85 | | D5 | 371.6 | 366.1 | 1.48 | | Arithmetic mean | ā | ā | 1.06 |
|
|