Mechanical and Durability Properties of Induction-Furnace-Slag-Incorporated Recycled Aggregate Concrete
Table 4
Slump value for concrete with different IFS ratio.
| | Sl. no. | IFS (%) | Strength (MPa) | Practical slump value in mm |
| | 1 | 0 | 17.23 | 45 | | 2 | 0 | 20.68 | 46 | | 3 | 0 | 24.13 | 48 | | 4 | 25 | 17.23 | 39 | | 5 | 25 | 20.68 | 30 | | 6 | 25 | 24.13 | 41 | | 7 | 50 | 17.23 | 32 | | 8 | 50 | 20.68 | 32 | | 9 | 50 | 24.13 | 34 | | 10 | 75 | 17.23 | 35 | | 11 | 75 | 24.13 | 31 | | 12 | 75 | 3500 | 30 | | 13 | 100 | 17.23 | 30 | | 14 | 100 | 20.68 | 32 | | 15 | 100 | 24.13 | 34 |
|
|