Research Article

Mechanical Properties and Thermal Conductivity of Aerogel-Incorporated Alkali-Activated Slag Mortars

Table 7

MIP test results of aerogel-incorporated AAS mortars.

Mix numberMedian pore diameter-area (nm)Median pore diameter-volume (nm)Total porosity (%)

S18.842.311.46
S2639.415.53
S35.839.515.48
S46.632.713.60