Research Article
Lightweight Cement Mortars with Granulated Foam Glass and Waste Perlite Addition
| Sample | GFG (g) | Cement CEM I 42.5R (g) | GFG/binder ratio | Ground expanded perlite (g) | Sand (g) | Water (g) | Superplasticizer (g) |
| 0.6/0-P | 270 | 450 | 0.6 | 90 | — | 225 | — | 0.6/0-0 | 270 | 450 | 0.6 | 0 | — | 225 | — | 0.9/0-P | 405 | 450 | 0.9 | 90 | — | 225 | 1.13 | 0.9/0-0 | 405 | 450 | 0.9 | 0 | — | 225 | 1.13 | 1.2/0-P | 540 | 450 | 1.2 | 90 | — | 225 | 2.25 | 1.2/0-0 | 540 | 450 | 1.2 | 0 | — | 225 | 2.25 | 0.6/S-P | 217 | 450 | 0.6 | 90 | 180 | 225 | — | 0.6/S-0 | 217 | 450 | 0.6 | 0 | 180 | 225 | — | 0.9/S-P | 314 | 450 | 0.9 | 90 | 260 | 225 | 1.13 | 0.9/S-0 | 314 | 450 | 0.9 | 0 | 260 | 225 | 1.13 | 1.2/S-P | 443 | 450 | 1.2 | 90 | 367 | 225 | 2.25 | 1.2/S-0 | 443 | 450 | 1.2 | 0 | 367 | 225 | 2.25 |
|
|