Lightweight Cement Mortars with Granulated Foam Glass and Waste Perlite Addition
Table 3
Content of active oxides in relation to the perlite grain size.
| Expanded perlite | SiO2(act) (%) | Al2O3(act) (%) | Sum of active oxides (%) |
| Normal < 1 mm | 17.0 | 2.8 | 19.8 | Waste powder < 100 µm | 31.1 | 5.5 | 36.6 | Ground waste powder < 10 µm | 48.2 | 6.6 | 54.8 |
|
|