Research Article
Effect of Warm-Mix Agent EC-120 on Performance of Asphalt Binder and Its Microscopic Mechanism
Table 1
Technical indexes of ESSO A-70 matrix asphalt.
| | Technical indexes | Unit | Results | Specification |
| | Penetration (25°C, 5 s, 100 g) | 0.1 mm | 67 | 60–80 | | Softening point | °C | 47.5 | ≥47 | | Ductility @15°C | cm | >100 | ≥100 | | Relative density @25°C | | 1.043 | Measured | | After TFOT | | | | | Mass changes | % | 0.1 | ±0.8 | | Residual penetration ratio (25°C, 5 s, 100 g) | % | 65.2 | ≥63 | | Residual ductility (5°C, 5 cm/min) | cm | 6.8 | ≥6 |
|
|