Research Article

Strength of Hollow Compressed Stabilized Earth-Block Masonry Prisms

Table 6

Flexural strength tests results for HCCSEBs with strength grade MU7.5.

NumberFlexural strength (MPa)Mean value (MPa)Mean coefficient of variation (%)

Group 7.5T-10.5∼0.60.588.63
Group 7.5T-20.5∼0.6
Group 7.5T-30.5∼0.6
Group 7.5T-40.5∼0.6
Group 7.5T-50.5∼0.7
Group 7.5T-60.5∼0.7