Research Article
Experimental Study on the Saturated Compacted Loess Permeability under K0 Consolidation
Figure 6
Relationship between the saturated permeability coefficient and the initial dry density under confining pressure consolidation. (a) σ3 = 100 kPa. (b) σ3 = 200 kPa. (c) σ3 = 300 kPa. (d) σ3 = 400 kPa.
(a) |
(b) |
(c) |
(d) |