Research Article
Ecological Upgrade of Normal-Strength Mortars by Using High Volume of GGBS
| | Groups | Curing conditions | | GGBS | Cement | Water | Sand |
| | Con | 23 ± 2°C >95% RH | 0.45 | 0 | 41. 40 | 18.60 | 40.00 | | C20T23W45 | 8.28 | 33.12 | 18.60 | 40.00 | | C10T23W45 | 4.14 | 37.26 | 18.60 | 40.00 | | C15T23W45 | 6.21 | 35.19 | 18.60 | 40.00 | | C25T23W45 | 10.35 | 31.05 | 18.60 | 40.00 | | C30T23W45 | 12.42 | 28.98 | 18.60 | 40.00 | | C20T40W45 | 40 ± 2°C >95% RH | 8.28 | 33.12 | 18.60 | 40.00 | | C20T60W45 | 60 ± 2°C >95% RH | 8.28 | 33.12 | 18.60 | 40.00 |
| | C20T23W35 | 23 ± 2°C | 0.35 | 8.89 | 35.55 | 15.55 | 40.00 | | C20T23W55 | >95% RH | 0.45 | 7.74 | 30.97 | 21.29 | 40.00 |
|
|