Research Article
Effect of Hybrid Steel-Basalt Fiber on Behaviors of Manufactured Sand RPC and Fiber Content Optimization Using Center Composite Design
Table 4
Physical and chemical properties of mineral powder.
| Properties | Standard value | Actual value |
| Physical properties | Specific surface area (m2/kg) | ≥400 | 429 | Liquidity ratio (%) | ≥95 | 102 | Density (%) | ≥2.8 | 2.8 |
| Chemical properties | Moisture content (%) | ≤1.0 | 1.0 | Loss on ignition (%) | ≤3.0 | 3.0 | Pozzolanic activity index (%) | 7 days ≥ 75 | 83 | 28 days ≥ 95 | 98 |
|
|