Research Article
Novel Approach to Handling Microfiber-Rich Dye Effluent for Sustainable Water Conservation
Table 1
Property of coagulant fly ash and ordinary Portland cement.
| S. no. | Description | OPC | Coagulant fly ash |
| 1 | Specific gravity | 3.21 | 2.23 | 2 | SiO2 | 20.28 | 59.73 | 3 | Al2O3 | 5.72 | 29.67 | 4 | Fe2O3 | 2.71 | 0.96 | 5 | CaO | 62.75 | 1.21 | 6 | MgO | 2.48 | 1.34 | 7 | SO3 | 1.92 | 4.52 | 8 | N2O | 0.19 | 0.43 | 9 | K2O | 0.84 | 1.19 |
|
|