Research Article
Development of Reinforcement Grout Materials Based on Blast Furnace Slag according to the Content of Reinforcement Fiber
Figure 5
Analysis of uniaxial compressive strength by C : B mixing ratios: (a) results of uniaxial compression test from nontreated specimen; (b) results of uniaxial compression test for O : A = 1.2 : 0.5%; (c) results of uniaxial compression test for O : A = 1.2 : 1.0%; (d) results of uniaxial compression test for C = 0.5%; (e) results of uniaxial compression test for C = 1.0%.
(a) |
(b) |
(c) |
(d) |
(e) |