Research Article

Development of Reinforcement Grout Materials Based on Blast Furnace Slag according to the Content of Reinforcement Fiber

Figure 6

Analysis of uniaxial compressive strength by fiber contents: (a) results of uniaxial compressive test for OPC : B = 100 : 0%; (b) results of uniaxial compressive test for OPC : B = 70 : 30%; (c) results of uniaxial compressive test for OPC : B = 40 : 60%.