Mixing ratio for measurement of uniaxial compression strength of grout materials using aramid fiber.

AB liquidFiber
SandOPCSlagCa(OH)2WaterOiling agent (%)Aramid
(g)(g)(ml)(ml)(g)

3507000500.70%
(100%)(0%)
492121290.35
(70%)(30%)1.2(0.5%)
28424280.7
(40%)(60%)(1.0%)