Research Article

Development of Reinforcement Grout Materials Based on Blast Furnace Slag according to the Content of Reinforcement Fiber

Table 3

Mixing ratio for measurement of uniaxial compression strength of grout materials using carbon fiber.

AB liquidFiber
Sand (g)OPCSlagCa(OH)2WaterCarbon
(g)(g)(ml)(ml)(g)

3507000500%
(100%)(0%)
492121290.35
(70%)(30%)(0.5%)
28424280.7
(40%)(60%)(1.0%)