Mechanical Properties Test and Strength Prediction on Basalt Fiber Reinforced Recycled Concrete
Table 5
Comparison of strength predictive and measured values of BFRRC.
| Sample name | Compressive strength (MPa) | Splitting tensile strength (MPa) | Flexural strength (MPa) | Measured values | Predictive value | Predictive error (%) | Measured values | Predictive value | Prediction error (%) | Measured values | Predictive value | Predictive error (%) |
| BFRRC40-0.1 | 40.24 | 40.65 | 1.02 | 3.79 | 3.85 | 1.58 | 5.61 | 5.77 | 2.85 | BFRRC40-0.2 | 43.28 | 43.12 | −0.37 | 4.92 | 5.01 | 1.83 | 6.84 | 6.99 | 2.19 | BFRRC40-0.3 | 42.74 | 42.9 | 0.37 | 4.76 | 4.8 | 0.84 | 7.54 | 7.42 | −1.59 | BFRRC70-0.1 | 36.95 | 36.12 | −2.25 | 3.44 | 3.39 | −1.45 | 4.78 | 4.81 | 0.63 | BFRRC70-0.2 | 41.24 | 41.63 | 0.95 | 3.55 | 3.64 | 2.54 | 5.46 | 5.53 | 1.28 | BFRRC70-0.3 | 38.87 | 39.25 | 0.98 | 4.2 | 4.31 | 2.62 | 6.02 | 6.17 | 2.49 | BFRRC100-0.1 | 38.43 | 37.97 | −1.20 | 3.07 | 3.14 | 2.28 | 5.02 | 4.88 | −2.79 | BFRRC100-0.2 | 43.29 | 43.02 | −0.62 | 3.43 | 3.34 | −2.62 | 5.98 | 6.12 | 2.34 | BFRRC100-0.3 | 41.17 | 41.69 | 1.26 | 3.85 | 3.92 | 1.82 | 7.34 | 7.29 | -0.68 |
|
|