Research Article
The Role of Iron Tailing Powder in Ultra-High-Strength Concrete Subjected to Elevated Temperatures
Table 2
Composition analysis of raw materials (%).
| Specimens | CaO | SiO2 | Al2O3 | Fe2O3 | SO3 | MgO | Loss on ignition |
| Cement | 57.58 | 20.35 | 6.12 | 4.23 | 2.19 | 2.59 | 2.59 | Silica fume | 0.41 | 94.02 | 0.27 | 0.11 | 0.11 | 0.34 | 2.86 | Iron tailing powder | 12.12 | 51.85 | 11.24 | 9.34 | 0.41 | 4.86 | 2.41 |
|
|