Concrete mix proportions and 28-day compressive strength.

Strength gradeWater (kg/m3)Cement (kg/m3)Mineral powder (kg/m3)Fly ash (kg/m3)Sand (kg/m3)Coarse aggregate (kg/m3)Admixture (kg/m3)Coarse aggregate size (mm)fcm (MPa)

C50155373107538148815.335–2068.4