Research Article
New Anticracking Glass-Fiber-Reinforced Cement Material and Integrated Composite Technology with Lightweight Concrete Panels
Table 6
Maximum shrinkage strain values of various specimens.
| Category | Surface shrinkage strain value (GRC) | Internal shrinkage strain value (PLC) |
| T1 | — | 908.64 × 10−6 | T2 | 1594.30 × 10−6 | — | T3 | 703.91 × 10−6 | 914.76 × 10−6 | T4 | 731.48 × 10−6 | 897.20 × 10−6 | T5 | 791.74 × 10−6 | 684.33 × 10−6 | T6 | 780.23 × 10−6 | 773.57 × 10−6 |
|
|