Research Article
Workability and Compressive Strength Behavior of a Cemented High-Porosity Backfill Material
Table 2
Summary of the mixture composition of the samples.
| | Group | Sample | Solid content (wt. (%)) | Solid content proportions | Density class (kg·m−3) | Silica fume in binder (wt. (%)) | | Binder (%) | Surface sand (%) |
| | A | 1 | 82.1 | 22.2 | 77.8 | 1000 | 10 | | 2 | 83.7 | 22.2 | 77.8 | 1000 | 10 | | 3 | 85.3 | 22.2 | 77.8 | 1000 | 10 | | 4 | 87.0 | 22.2 | 77.8 | 1000 | 10 |
| | B | 5 | 83.7 | 25 | 75 | 1000 | 10 | | 6 | 83.7 | 22.2 | 77.8 | 1000 | 10 | | 7 | 83.7 | 20 | 80 | 1000 | 10 | | 8 | 83.7 | 18.2 | 81.8 | 1000 | 10 |
| | C | 9 | 83.7 | 22.2 | 77.8 | 1000 | 0 | | 10 | 83.7 | 22.2 | 77.8 | 1000 | 5 | | 11 | 83.7 | 22.2 | 77.8 | 1000 | 10 | | 12 | 83.7 | 22.2 | 77.8 | 1000 | 15 |
| | D | 13 | 83.7 | 22.2 | 77.8 | 600 | 10 | | 14 | 83.7 | 22.2 | 77.8 | 800 | 10 | | 15 | 83.7 | 22.2 | 77.8 | 1000 | 10 | | 16 | 83.7 | 22.2 | 77.8 | 1200 | 10 | | 17 | 83.7 | 22.2 | 77.8 | 1400 | 10 | | 18 | 83.7 | 22.2 | 77.8 | 1600 | 10 |
|
|