Study on Properties of Drainage SBS Modified Asphalt Mixture with Fiber

Table 1

Technical indicators of 70 matrix asphalt.

Test metricTest resultSpecification requirementTest method

Needle penetration (25°C, 100 g, 5 s) (0.1 mm)68.260∼80T0604
Softening point (ball and ring method) (°C)57.2≥46.0T0606
Ductility (5 cm/min, 15°C) (cm)106.3≥100T0605
Flash point (°C)268≥260T0611
Density (g·cm−3)1.025Actual measurementT0603
Solubility (%)99.7≥99.5T0607
After RTFOTMass variation (%)−0.1−0.8∼+0.8T0610
Penetration ratio (%)72.1≥61T0604
Ductility (5 cm·min−1, 15°C) (cm)7≥6T0605