Research Article
Axial Loading Behaviour of Self-Compacting Concrete-Filled Thin-Walled Steel Tubular Stub Columns
Table 2
Mix proportion of self-compacting concrete.
| Type of concrete | Water (kg·m−3) | Cement (kg·m−3) | Fine aggregates (kg·m−3) | Coarse aggregates (kg·m−3) | Fly ash (kg·m−3) | Superplasticizer (%) |
| Self-compacting | 198.96 | 401.47 | 836.46 | 768.5 | 122.1 | 0.4 |
|
|