Study on the Water-Physical Properties of the Cement-Plaster Bonded Rock-Like Materials
Table 4
Orthogonal experiment results of the similar material ratio.
| Number | Water absorption (%) | Softening coefficient ηc | Permeability coefficient k (10−5 cm/s) | I | II | III | Mean | I | II | III | Mean | I | II | III | Mean |
| 1 | 15.1 | 16.2 | 16.1 | 15.8 | 0.477 | 0.482 | 0.469 | 0.476 | 0.098 | 0.256 | 0.132 | 0.162 | 2 | 17.6 | 17.8 | 18.6 | 18.0 | 0.505 | 0.498 | 0.503 | 0.502 | 0.355 | 0.398 | 0.453 | 0.402 | 3 | 18.8 | 19.6 | 19.2 | 19.2 | 0.633 | 0.641 | 0.64 | 0.638 | 4.068 | 4.003 | 3.824 | 3.965 | 4 | 21.1 | 20.8 | 19.6 | 20.5 | 0.708 | 0.701 | 0.703 | 0.704 | 10.085 | 8.987 | 8.624 | 9.232 | 5 | 21.5 | 20.2 | 21.3 | 21.0 | 0.506 | 0.503 | 0.494 | 0.501 | 0.878 | 0.968 | 0.926 | 0.924 | 6 | 13.2 | 14.5 | 13.1 | 13.6 | 0.589 | 0.581 | 0.579 | 0.583 | 0.312 | 0.485 | 0.391 | 0.396 | 7 | 22.2 | 21.8 | 22.9 | 22.3 | 0.601 | 0.605 | 0.600 | 0.602 | 28.069 | 29.622 | 31.268 | 29.653 | 8 | 19.8 | 20.8 | 19.7 | 20.1 | 0.622 | 0.618 | 0.629 | 0.623 | 8.658 | 7.652 | 7.285 | 7.865 | 9 | 26.1 | 27.1 | 26.3 | 26.5 | 0.441 | 0.451 | 0.446 | 0.446 | 9.712 | 10.989 | 9.134 | 9.945 | 10 | 30.5 | 30.1 | 30.3 | 30.3 | 0.481 | 0.485 | 0.498 | 0.488 | 38.956 | 39.861 | 41.339 | 40.052 | 11 | 13.0 | 14.1 | 13.4 | 13.5 | 0.628 | 0.633 | 0.635 | 0.632 | 0.751 | 0.621 | 0.584 | 0.652 | 12 | 16.8 | 16.9 | 17.9 | 17.2 | 0.712 | 0.725 | 0.702 | 0.713 | 1.389 | 1.847 | 1.687 | 1.641 | 13 | 30.0 | 31.0 | 29.9 | 30.3 | 0.415 | 0.42 | 0.428 | 0.421 | 49.698 | 41.295 | 48.846 | 46.613 | 14 | 26.5 | 26.8 | 27.7 | 27.0 | 0.556 | 0.543 | 0.551 | 0.550 | 13.369 | 12.087 | 12.803 | 12.753 | 15 | 20.1 | 21.1 | 20.9 | 20.7 | 0.561 | 0.568 | 0.557 | 0.562 | 2.611 | 2.148 | 2.945 | 2.568 | 16 | 16.6 | 16.5 | 15.8 | 16.3 | 0.687 | 0.692 | 0.691 | 0.690 | 0.772 | 0.821 | 0.948 | 0.847 |
|
|