Research Article

Analysis on the Strength of Cement Mortar Mixed with Construction Waste Brick Powder

Table 6

Grey entropy of mortar strength activity index and BP particle distribution.

Strength activity index<1 μm10∼20 μm20∼40 μm40∼60 μm>60 μm

Compressive strength (MPa)7 d0.99560.97270.94610.88130.8113
28 d0.99970.98540.93800.87690.8113
Flexural strength (MPa)7 d0.99780.97830.94270.87940.8113
28 d1.00000.98900.93520.87540.8113