Research on Corrosion Damage and Bearing Characteristics of Bridge Pile Foundation Concrete under a Dry-Wet-Freeze-Thaw Cycle

Table 6

Regression equations of the antierosion coefficient at different depths.

LocationRegression equation and R2

Water,
Surface,
0.25 m underground,
1.25 m underground,