Strength and Road Performance of Superabsorbent Polymer Combined with Cement for Reinforcement of Excavated Soil
Table 6
CBR values of representative samples.
| Symbol | 7 d CBR (%) | 28 d CBR (%) |
| Unstabilized | 3.5 | 3.8 | C2 | 7.2 | 10.1 | C4 | 12.0 | 19.2 | C6 | 15.2 | 35.7 | C2S15 | 6.8 | 9.4 | C2S30 | 6.1 | 8.6 | C2S45 | 5.5 | 8.1 | C4S15 | 11.2 | 18.1 | C4S30 | 9.8 | 17.3 | C4S45 | 8.7 | 15.8 | C6S15 | 13.9 | 32.8 | C6S30 | 12.3 | 30.1 | C6S45 | 10.7 | 27.7 |
|
|