Research Article
Rutting Resistance of Hot Mix Asphalt Containing Coarse Recycled Concrete Aggregates Coated with Waste Plastic Bottles
Table 5
Parameters of the Francken model.
| | Temperatures | Specimens | Parameters | | A | B | C | D |
| | 40°C | Control | 0.302 | 0.332 | 0.187 | 0.00022 | | 15% CRCA | 0.306 | 0.351 | 0.162 | 0.00027 | | 15% CRCA + WPB | 0.305 | 0.342 | 0.170 | 0.00024 | | 30% CRCA | 0.313 | 0.385 | 0.144 | 0.00035 | | 30% CRCA + WPB | 0.311 | 0.361 | 0.173 | 0.00029 | | 50% CRCA | 0.175 | 0.504 | 0.032 | 0.00066 | | 50% CRCA + WPB | 0.204 | 0.463 | 0.027 | 0.00053 |
| | 60°C | Control | 0.297 | 0.355 | 0.488 | 0.00042 | | 15% CRCA | 0.306 | 0.383 | 0.465 | 0.00053 | | 15% CRCA + WPB | 0.301 | 0.362 | 0.476 | 0.00047 | | 30% CRCA | 0.413 | 0.397 | 0.492 | 0.00082 | | 30% CRCA + WPB | 0.302 | 0.377 | 0.418 | 0.00068 | | 50% CRCA | 0.383 | 0.439 | 0.621 | 0.0025 | | 50% CRCA + WPB | 0.434 | 0.407 | 0.515 | 0.0012 |
|
|