Research Article
Influence of Steel Slag-Superfine Blast Furnace Slag Composite Mineral Admixture on the Properties of Mortar and Concrete
Figure 1
Compressive strength of pure cement mortar and composite admixture mortar (w/s ratio is 0.5). The total content of composite admixture is (a) 20% and (b) 30%.