Mix proportion (w/s is 0.5) of mortar containing composite mineral admixture for compressive strength test (kg).

GroupCementSSSBFSSandWater

C1450001350225
S1-20%360819
S2-20%76.513.5
S3-20%7218
S4-20%67.522.5
S1-30%315121.513.5
S2-30%114.720.3
S3-30%10827
S4-30%101.233.8