Mix proportion of concrete containing composite mineral admixture for compressive strength test (kg/m3).

GradeGroupw/sCementSSSBFSSandAggregateWater

C30S-10.47200120307801035165
S-2112.537.5
S-30.45175145357901025161
S-4131.243.8

C40SS-10.395250120307301055158
SS-2112.537.5
SS-30.385200160407201070154
SS-415050