Research Article

Influence of Steel Slag-Superfine Blast Furnace Slag Composite Mineral Admixture on the Properties of Mortar and Concrete

Table 6

Mix proportion of self-compacting concrete containing composite mineral admixture (kg/m3).

GradeGroupw/sCementSSSBFSSandAggregateWater

C50Z10.3134012832810890157
Z212040

C60ZZ10.27838014436780880156
ZZ213545