Research Article

Resilient Performance of Self-Centering Hybrid Rocking Columns: Theory, Experiment, and Numerical Simulation

Table 7

The maximum deformation, residual deformation, and self-centering capacity coefficients in each test working case.

Case numberMaximum deformation, Δmax (mm)Residual deformation, Δc (mm)Self-centering capability factor, γ (%)

Specimen 163.213.2194.92
Specimen 267.097.0689.47
Specimen 364.126.7789.44
Specimen 464.756.0290.70
Specimen 564.189.1185.81
Specimen 664.154.4993.00
Specimen 766.2038.5641.75