Research Article

Research and Model Prediction on the Performance of Recycled Brick Powder Foam Concrete

Table 10

Analysis of extreme differences in compressive strength of ordinary foam concrete.

 Bubble volumesWater cement ratio

K12.041.56
K21.421.65
K31.391.69
K41.271.27
K51.121.08
Extreme difference value R0.920.61
Rank12