Orthogonal test factor level of experimental group.

LevelFactor
Bubble volumes (A) (%)Recycled brick powder volume (B) (%)Water to material ratio (C) (%)HPMC content (D)

13100.450.03
24200.50.04
35300.550.05
46400.60.06
57500.650.07