Orthogonal test results of recycled brick powder foam concrete.
| Group number | Dry density (kg/m3) | 28 d compressive strength (MPa) | Specific strength (N·m·kg−1) | Group number | Dry density (kg/m3) | 28 d compressive strength (MPa | Specific strength (N·m·kg−1) |
| 1 | 1171.10 | 6.07 | 5185.30 | 14 | 710.85 | 0.84 | 1186.89 | 2 | 1210.25 | 5.80 | 4792.61 | 15 | 838.75 | 2.37 | 2830.70 | 3 | 988.00 | 5.76 | 5833.35 | 16 | 806.80 | 2.11 | 2621.41 | 4 | 1072.75 | 4.55 | 4241.30 | 17 | 952.50 | 2.82 | 2955.64 | 5 | 1039.45 | 3.09 | 2975.81 | 18 | 857.60 | 2.47 | 2882.64 | 6 | 997.15 | 5.17 | 5183.17 | 19 | 647.65 | 1.74 | 2686.56 | 7 | 854.25 | 4.23 | 4947.38 | 20 | 889.40 | 1.25 | 1404.43 | 8 | 680.85 | 3.11 | 4570.76 | 21 | 769.50 | 2.15 | 2794.67 | 9 | 937.55 | 2.26 | 2410.22 | 22 | 975.85 | 2.58 | 2645.59 | 10 | 1071.20 | 3.04 | 2838.83 | 23 | 851.15 | 1.51 | 1777.36 | 11 | 988.20 | 5.31 | 5369.92 | 24 | 675.20 | 1.96 | 2901.14 | 12 | 1008.45 | 2.76 | 2736.92 | 25 | 786.60 | 0.96 | 1226.04 | 13 | 721.45 | 1.46 | 2020.72 | | | | |
|
|