Research Article
Axial Compression Behavior of Recycled Concrete Filled Steel Tubular Short Columns after High Temperature
Table 2
Content of each component and measured strength of recycled concrete.
| Substitutionrate (%) | Concrete material consumption (kg/m3) | Cube compressive strength of specimen (MPa) | Cement | Recycled coarseaggregate | Fineaggregate | Water (kg/m3) | Test piece 1 | Test piece 2 | Test piece 3 | Average value |
| 100 | 550 | 1221 | 575 | 154 | 59.87 | 25.81 | 37.07 | 38.25 |
|
|