Research Article
Characteristic Evolution of GO/SBS-Modified Asphalt during Aging
Table 3
Physical characteristics of SBS-T6302.
| | Item | Unit | Measured value |
| | Volatile | % | 0.38 | | 300% stretching stress | MPa | 2.41 | | Tensile strength | MPa | 26.8 | | Elongation at break | % | 735 | | Shore hardness | HA | 81 |
|
|