Research Article
Mechanical and Durability Performance of High-Strength Concrete with Waste Tyre Steel Fibres
Figure 7
Chloride ion penetration. (a) Weighed silver nitrate powder. (b) 0.1 M silver nitrate solution. (c) Chloride ion penetration depth for CM after curing for 28 days in NaCl solution. (d) Chloride ion penetration depth for SFRC30-0.75 after curing for 28 days in NaCl solution.
(a) |
(b) |
(c) |
(d) |