Research Article
Shield Cutting Pile-Group Implementation Effects on the Superstructure
Table 3
Secondary grouting slurry ratio table.
| | 
 |  | Material name | Material parameters | Proportion | Coagulation time (s) | 28 days strength (Mpa) |  | 
 |  | Cement | P.O 42.5 | Water : Water glass : Cement slurry = 3 : 1:1 (volume ratio) | 30 | 2.6 |  | Water glass | Baumé degree: 30∼35, modulus: 2.8∼3.1 |  | 
 | 
 |