Carbonation Characteristics and Bearing Capacity Attenuation of Loaded RC Beam Coupled with Chloride Erosion

Table 2

Mix proportion of concrete and compressive/tensile strength.

Concrete gradeCement (kg/m3)Water (kg/m3)Sand (kg/m3)Crushed stone (kg/m3)Admixture (kg/m3)Compressive strength fc (MPa)Tensile strength ft (MPa)

C4042616276310148.543.051.20
C5049016259412068.854.041.32