Research Article

Optimization Analysis of Mechanical Properties of Fly Ash-Based Multicontent Gasification Slag Paste Filling Material

Table 2

Response surface design and results.

No.LevelEarly compressive strength (MPa)No.LevelEarly compressive strength (MPa)
X1X2X3X43 d7 d14 dX1X2X3X43 d7 d14 d

1−1−1000.5440.8682.41601101.4042.1733.3
21−1000.5880.7041.217−10−101.3801.6732.6
3−11001.2521.8772.31810−101.0161.2001.8
411001.4682.1533.519−10100.9361.0321.2
500−1−11.0802.1413.12010100.7400.8440.9
6001−10.9081.5483.5210−10−10.7360.8480.9
700−111.0321.9293.122010−10.9921.0922.1
800110.7481.2322.6230−1011.5882.5612.6
9−100−11.2562.1974.12401011.4602.1572.2
10100−10.9201.2041.82500000.8761.2361.9
11−10011.0881.3481.52600000.9321.3121.5
1210010.6560.8121.12700000.7641.1801.7
130−1−100.7120.7601.22800000.9841.1641.6
1401−101.0721.7533.02900000.9761.3041.6
150−1100.6400.6080.8Response surface design method-central combination design method