The Impact of Molar Proportion of Sodium Hydroxide and Water Amount on the Compressive Strength of Slag/Metakaolin (Waste Materials) Geopolymer Mortar

Figure 4

The impact of superplasticiser and low water amount on compressive strengths at 7 curing days.