Research Article

Corrosion Zones of Rebar in High-Volume Fly-Ash Concrete through Potentiodynamic Study in Concrete Powder Solution Extracts: A Sustainable Construction Approach

Table 4

Icorr (μA/cm2) for carbonated CPSE for various types of steel and different fly-ash content with water-binder ratios.

Steel typeCRSTata TMTLocal TMT
% FA contentw/bw/bw/b
0.350.400.450.350.400.450.350.400.45

01.31.72.11.81.91.92.22.83.1
201.21.82.31.91.61.82.13.43.9
401.21.42.31.51.52.41.62.53.6
500.91.51.91.31.52.222.52.8
601.82.42.82.02.53.02.222.4
702.22.53.12.62.73.12.53.84.3