[Retracted] Experimental Study on Mineral Solid Waste Green Grouting Material Based on Electromagnetic Characteristic Detection
Table 1
Cement properties content and other natural requirements.
| Chemical composition | SiO2 | Fe2O3 | Al2O3 | CaO | MgO | SO3 | Loss |
| Content (%) | 22.63 | 3.83 | 5.71 | 58.95 | 1.89 | 2.62 | 4.37 |
| | Chemical composition content (%) | Specific surface area | Water requirement of normal consistency (%) | Setting time (min) | Flexural strength (MPa) | Compressive strength (MPa) | Loss | MgO | SO3 | m2/kg | Initial setting | Final setting | 3 d | 28 d | 3 d | 28 d | Index requirements | ≤5.0 | ≤5.0 | ≤3.5 | ≥300 | | ≥45 | ≤600 | ≥3.5 | ≥6.5 | ≥17.0 | ≥42.5 | Experimental data | 4.37 | 1.89 | 2.62 | 354 | 27.5 | 182 | 235 | 5.7 | 7.8 | 31.5 | 56.9 | Single evaluation | Standard | Standard | Standard | Standard | Standard | Standard | Standard | Standard | Standard | Standard | Standard |
|
|