Research Article
Road Performance and Ice-Melting Characteristics of Steel Wool Asphalt Mixture
| Technical index | Unit | Requirement | Test value | Testing standard |
| Penetration (25°C, 5 s, 100 g) | 0.1 mm | 40–60 | 58 | T0604-2011 | Penetration index | — | ≥0 | 0.035 | T0604-2011 | Softening point | °C | ≥60 | 68 | T0606-2011 | Ductility (5oC) | cm | ≥20 | 31 | T0605-2011 | Brookfield viscosity (60oC) | Pa·s | ≤3.0 | 2.13 | T0625-2011 | Elastic recovery (25oC) | cm | ≥75 | 78.0 | T0662-2000 | Flash point | °C | ≥230 | 296.8 | T0611-2011 | Storage stability | °C | ≤2.5 | 2.0 | T0611-2011 | Rolling thin film oven test | Quality change | % | ±1.0 | −0.150 | T0609-2011 | Penetration ratio | % | ≥65 | 77.2 | T0604-2011 | Ductility (5 cm/min, 10°C) | cm | ≥15 | 16 | T0605-2011 |
|
|